EN 1670

Corrosion resistance shall be classified according to the following grading system:

Grade

Corrosion resistance

Neutral salt spray test

0

no defined

-

-

1

low

24 h

-0/+1h

2

moderate

48 h

-0/+1h

3

high

96 h

-0/+1h

4

very high

240 h

-0/+1h

5

exceptionally high

480 h

-0/+1h

EN 13126-3

Durability shall be classified according to the following grading system:

Grade

Cycles

3/90

10.000 Turn-Only

4/90

15.000 Turn-Only

5/90

25.000 Turn-Only

3/180

10.000 Tilt&Turn

4/180

15.000 Tilt&Turn

5/180

25.000 Tilt&Turn

EN 13126-8:2006

Durability shall be classified according to the following grading system:

Grade

Cycles

4

15.000

5

25.000

EN 1154

Durability shall be classified according to the following grading system:

Grade

Cycles

8

500.000

EN 13126-1 & 13126-9 & EN 13126-15 & EN 13126-16:2008

Durability shall be classified according to the following grading system:

Grade

Cycles

3

10.000

4

15.000

5

25.000

Corrosion resistance shall be classified according to EN 1670